$30.50
$61.00
50% OFF! Hot items selling fast—Grab them before they're gone!
C/4-C/6
Plastic clay for wheel and modeling. Granular manganese give speckled surface. Ideal temperature for best color is C/5. Good in oxidation or reduction firing.
C/4 AverageShrinkage 10.5% Absorption 4.5%
C/6 AverageShrinkage 11.0% Absorption 2.25%
Product Number: 10112
**In dry form it is recommended to use a respirator because of the manganese.**